Packaging Quality Issue & Solutions XVIIII

Return list

Packaging Quality Issue & Solutions XVIIII

Nov 11,2026
问:The flexible packaging was punctured by internal sharp corners or external hard objects, and the standardized puncture strength did not meet the requirements.

答:

The flexible packaging of bone-in cooked foods, nut shells, frozen block-shaped foods, etc., may be punctured by the sharp corners of the contents or external hard objects during transportation vibration or stacking compression, resulting in holes and causing air leakage and leakage of liquids. Although Scheme 28 mentioned puncture tests previously, it did not refer to the specific puncture strength national standard for plastic films, and the basis for judgment was not clear.

 

Solution:

 

  1. Standardized puncture strength test: According to GB/T 37841-2019 "Test Method for Puncture Resistance of Plastic Films and Sheets", use a puncture strength tester to make the standard probe penetrate the film sample vertically at a specified speed, and record the maximum force value (N) required for penetration. This standard is clearly applicable to soft plastic films and sheets with a thickness of less than 1mm.The test can be conducted by the customized tensile tester (https://www.linktesting.org/7007.html/automatic-tensile-tester-xlw-500n/)
  2. Puncture verification of finished bags: Conduct puncture tests on finished soft packaging bags (not only the film sample) to more accurately reflect the puncture resistance of the bag under actual usage conditions and evaluate the integrity of the packaging overall structure.

问:The heat sealing strength was qualified upon leaving the factory, but it significantly decreased after being stored at high temperatures, resulting in a slight opening of the seal.

答:

The heat sealing strength of the flexible packaging was within the acceptable range during the factory inspection. However, after being stored for several weeks in a high-temperature warehouse or container in summer, the sealing strength significantly decreased (there are cases showing that after storage at 60℃ for 14 days, the strength dropped from 1.5 N/15mm to 0.3 N/15mm), resulting in slight opening of the seal, microbial invasion or oxidation of the contents. And the regular factory inspection cannot detect this hidden danger.

 

Solution:

 

  1. Heat sealing strength attenuation test: Place the heat-sealed sample in a high-temperature and high-humidity aging chamber, and leave it under the specified conditions (such as 60℃ or 40℃/75%RH) for a certain period of time (7 days, 14 days). After removal, let it balance in the standard environment, and then test the heat sealing strength using an electronic tensile testing machine, calculating the retention rate of strength. If the retention rate is lower than 80%, it is determined that the sealing reliability of the shelf life is insufficient.The test can be conducted by the tensile tester(https://www.linktesting.org/7007.html/automatic-tensile-tester-xlw-500n/) and temperature and humidity control chamber.
  2. Comparison of attenuation under different heat sealing parameters: For the sample groups prepared from the same material under different heat sealing temperatures/pressures/durations, conduct strength tests after aging simultaneously. Identify the "initial strength is qualified and the attenuation is the slowest" heat sealing process window, rather than merely pursuing the highest factory strength.
  3. Simultaneous assessment of peel strength attenuation: The inter-layer peel strength of the composite film may also attenuate after aging. Simultaneous testing can distinguish whether it is the failure of the heat sealing layer or the failure of the composite layer.

问:After steaming, the adhesion of the bag significantly decreases, and there is layer separation. However, the test results before steaming were qualified.

答:

After being sterilized at 121℃, the retort pouches exhibited interlayer separation and delamination. However, the peel strength test before sterilization was qualified. The core of the resistance to sterilization lies not only in "meeting the standards before sterilization", but also in "maintaining the standards after sterilization". The insufficient temperature resistance of the adhesive is the main cause.

 

Solution:

  1. Comparison test of peel strength before/after cooking: According to GB/T 41168-2021 "Plastic and Aluminum Foil Steam-Processed Composite Films and Bags for Food Packaging" or GB/T 10004-2008, the interlayer peel strength was tested before and after the cooking process (121℃×30min or according to the product process). The retention rate of peel strength after cooking is the core indicator for determining the resistance to cooking.The test can be conducted by the tensile tester (https://www.linktesting.org/7007.html/automatic-tensile-tester-xlw-500n/).
  2. Test of post-cooking heat sealing strength: Simultaneously test the heat sealing strength of the sealed opening after cooking. For cooking bags, the retention rate of heat sealing strength is usually required to be ≥ 80%.
  3. Verification of sealing performance after cooking: Conduct negative pressure sealing test on the entire bag sample after cooking to check if there is leakage or rupture in the bag body and the sealing edge. Visual inspection is conducted for bubbling.The test can be conducted by the leak tester (https://www.linktesting.org/903.html/leakage-tester/).

问:The peel strength of the composite film is insufficient, but it is impossible to determine whether the problem lies in the adhesive or the surface treatment of the substrate.

答:

The composite film shows layering and has a low peel strength. Routine tests can only confirm that "the peel force does not meet the standard", but cannot determine whether it is due to incomplete curing of the adhesive, insufficient coating amount, or attenuation of the corona treatment on the substrate resulting in insufficient surface tension. Different root causes require completely different rectification directions. Blind adjustments to the process are often ineffective.

 

Solution:

  1. Observation of interface morphology and determination of failure mode: Conduct macroscopic inspection and microscopic observation on the two interfaces after peeling, and determine whether the failure mode is interface failure (complete separation of the adhesive layer from the substrate), cohesive failure (breakage of the adhesive layer itself), or mixed failure. Interface failure indicates problems on the substrate surface, while cohesive failure indicates problems with the adhesive's curing or formulation.
  2. Surface tension (dynes) test: Use a dynometer or contact angle measuring instrument to measure the surface tension of the corona surface of the failed batch and the normal batch of substrates. If the dynes value of the failed batch is significantly lower (such as below 38 mN/m), it indicates that the attenuation of corona treatment is the main cause of the peeling failure.
  3. Analysis of adhesive curing degree: Use infrared spectroscopy or DSC methods to evaluate whether the adhesive layer is fully cured and whether the crosslinking density is normal, ruling out the possibility of insufficient curing time or temperature.

问:The BOPP/PE film gets stuck after being wound up, and it is difficult to unwind the film or make an opening.

答:

Soft packaging films (especially the heat-sealing layers of BOPP, PE single-layer films or composite films) may stick together when being wound up, stored, or transported under high temperatures in summer. When unwound, they are difficult to separate. In mild cases, the opening may be obstructed or the film may deviate during unwinding. In severe cases, the film may break or the film surface may be damaged, causing the printing or bag-making processes to stop. Adhesion is an unintended inter-layer adhesion that occurs between film layers under the combined effects of pressure, temperature, and time. Unlike the friction coefficient, it reflects the ease or difficulty of the film layers to separate after static compression storage.

 

Solution:

  1. Anti-adhesion force (tear force) test: According to ASTM D3354 (parallel plate method) or relevant methods in GB/T 10003, place two film specimens in a stacked configuration under specified temperatures (such as 50°C or 60°C) and specified pressures for a certain period of time. After cooling, use a tensile testing machine to separate the two layers of film at a constant speed and record the maximum force required for separation (in grams or Newtons), which is the anti-adhesion force. The lower the anti-adhesion force, the better the film's anti-adhesion performance.The test can be conducted by the tensile tester(https://www.linktesting.org/7007.html/automatic-tensile-tester-xlw-500n/)
  2. Friction coefficient verification in combination: Simultaneously test the static/dynamic friction coefficients of the film. Films with severe adhesion often have a higher friction coefficient, but the two are not completely equivalent - the friction coefficient reflects dynamic smoothness, while the anti-adhesion force reflects the separation ability after static compression. They need to be judged separately.The test can be conducted by the COF tester (https://www.linktesting.org/936.html/coefficient-of-friction-tester-ltmxs-06/)

📩 Request a tailored test scheme for your product📩 获取针对您产品的定制测试方案

Response within 24 hours · Factory-direct quotation · ASTM / ISO compliant

Live Chat